I wouldn't trust anything but silver solder - braze it with oxy-acetalyne. This also demands pretty tight fitting tolerances. Clean joints and flux, and you should be good. Randy Bergum 1990 Carat
> [Original Message] > From: George Goff <THX0001@AOL.COM> > To: <vanagon@GERRY.VANAGON.COM> > Date: 10/16/2002 4:04:08 AM > Subject: ??? Solder Joint Design ??? > > I am fabricating a couple little doodads for my van's cooling system. Sounds > like a recipe for disaster, doesn't it? Since the joints will be unstressed, > I intend to use SOFT, silver bearing solder. Does anybody know what kind of > a fit, i.e., amount of gap, is needed in a socket to make a proper solder > joint? The material is brass and the tubing OD is about 3/8" (10 mm to you > younger guys). > > Thanks to one and all, |
Please note - During the past 17 years of operation, several gigabytes of
Vanagon mail messages have been archived. Searching the entire collection
will take up to five minutes to complete. Please be patient!
Return to the archives @ gerry.vanagon.com
The vanagon mailing list archives are copyright (c) 1994-2011, and may not be reproduced without the express written permission of the list administrators. Posting messages to this mailing list grants a license to the mailing list administrators to reproduce the message in a compilation, either printed or electronic. All compilations will be not-for-profit, with any excess proceeds going to the Vanagon mailing list.
Any profits from list compilations go exclusively towards the management and operation of the Vanagon mailing list and vanagon mailing list web site.