Vanagon EuroVan
Previous messageNext messagePrevious in topicNext in topicPrevious by same authorNext by same authorPrevious page (July 2017, week 1)Back to main VANAGON pageJoin or leave VANAGON (or change settings)ReplyPost a new messageSearchProportional fontNon-proportional font
Date:         Wed, 5 Jul 2017 20:50:41 +0000
Reply-To:     Patrick Seurynck <climb12@GMAIL.COM>
Sender:       Vanagon Mailing List <vanagon@gerry.vanagon.com>
From:         Patrick Seurynck <climb12@GMAIL.COM>
Subject:      Re: Poptop frame/catch refurb
Comments: To: Alistair Bell <albell@shaw.ca>
In-Reply-To:  <F9A646B0-FAB7-4A04-9425-E158FA55FFCE@shaw.ca>
Content-Type: text/plain; charset="UTF-8"

Alistair, On a minutely different subject, I ran across a writeup you had done, a while back, about rebuilding the hinged portion of the westy roof support mechanism and possibly creating a kit that could be purchased for that job. I have not taken mine apart to see what it needs but it is acting up. Have you created the rebuild kit? Patrick

On Wed, Jul 5, 2017 at 2:38 PM Alistair Bell <albell@shaw.ca> wrote:

> I've polished the galvey fittings, won't do that again. Apart from the > hazard of polishing zinc ( bad vapour/particles to breathe) it dulls again > pretty quickly. Mind you it did look sharp for a while. > > If I was to do it again I'd have them sandblasted and powdered. It's > expensive, well it is if you get a good company to do it, but it looks > cleaner. > > Aliatair > > > > On Jul 5, 2017, at 1:33 PM, Cunegonde <cunegonde.van.westfalia@GMAIL.COM> > wrote: > > > > Cunegonde has been in the Northwest her entire life since she was > imported. Needless to say there was the usual mildew farm in the lid > flocking, and corrosion on the pop top frame and lock. I also stripped, > cleaned and re-installed all the upholstery. Who knew it wasn't stripes > over camouflage pattern?! > > > > Now that the soft bits are cleaned, It's time to re-finish all of the > galvanized steel up there. I prefer to clean the galvanizing, and then use > a two-part epoxy paint that can handle lubricating the various joints & > bearing surfaces. Or should I go for powder coating - seems expensive for > interior pieces. > > > > What sayeth the list wisdom? > -- Sent from Gmail Mobile


Back to: Top of message | Previous page | Main VANAGON page

Please note - During the past 17 years of operation, several gigabytes of Vanagon mail messages have been archived. Searching the entire collection will take up to five minutes to complete. Please be patient!


Return to the archives @ gerry.vanagon.com


The vanagon mailing list archives are copyright (c) 1994-2011, and may not be reproduced without the express written permission of the list administrators. Posting messages to this mailing list grants a license to the mailing list administrators to reproduce the message in a compilation, either printed or electronic. All compilations will be not-for-profit, with any excess proceeds going to the Vanagon mailing list.

Any profits from list compilations go exclusively towards the management and operation of the Vanagon mailing list and vanagon mailing list web site.